<p>along the gauge length, depending on the standard used. Both ends of thespecimens should have sufficient length and a surface condition such that they are firmly grippedduring testing. The initial gauge length Lo is standardized (in several countries) and varies with thediameter (Do) or the cross-sectional area (Ao) of the specimen as listed</p>

<p><big>Equipment</big></p>
<p>The most common testing machine used in tensile testing is the <a href="page.php?w=universal_testing_machine">universal testing machine</a>. This type of machine has two crossheads;</p><p>
<a accesskey="1" href="page.php?w=tensile_testing&amp;p=9">1.Previous</a><br />
<a accesskey="3" href="page.php?w=tensile_testing&amp;p=11">3.Next</a>
</p>

<do type="prev" label="Search">
        <go href="search.wml"/>
</do>

</card>
</wml>