<p>different from oxide layers that are formed upon heating and are in the micrometer thickness range - the passive film recovers if removed or damaged whereas the oxide layer does not. Passivation in natural environments such as air, water and soil at moderate <a href="page.php?w=pH">pH</a> is seen in such materials as <a href="page.php?w=aluminium">aluminium</a>, <a href="page.php?w=stainless_steel">stainless steel</a>, <a href="page.php?w=titanium">titanium</a>, and <a href="page.php?w=silicon">silicon</a>.</p>

<p>Passivation is primarily determined</p><p>
<a accesskey="1" href="page.php?w=Corrosion&amp;p=15">1.Previous</a><br />
<a accesskey="3" href="page.php?w=Corrosion&amp;p=17">3.Next</a>
</p>

<do type="prev" label="Search">
        <go href="search.wml"/>
</do>

</card>
</wml>