<p>additional grinding at a smaller grit size can be done. Typically, two or three stages of grinding are used, with the second and third stages having a size that is decreasing. For example, a typical set of grit stages is 30 micrometer, then 15 micrometer, then 9 micrometer. An alternate set of typical grit stages is 20 micrometer, then 12 micrometer, then 5 micrometer.</p>

<p>Types of abrasives include <a href="page.php?w=aluminium_oxide">aluminium oxide</a>, industrial diamond, and <a href="page.php?w=silicon_carbide">silicon carbide</a>. Diamond</p><p>
<a accesskey="1" href="page.php?w=Optical_manufacturing_and_testing&amp;p=8">1.Previous</a><br />
<a accesskey="3" href="page.php?w=Optical_manufacturing_and_testing&amp;p=10">3.Next</a>
</p>

<do type="prev" label="Search">
        <go href="search.wml"/>
</do>

</card>
</wml>